Wood ash is generated as residual/waste from combustion done in boilers at pulp and paper mills, steam power plants, and other thermal power generating facilities. Since wood is a renewable resource for energy and an environmentally friendly material, there is an increased requirement of using waste wood for the purpose of energy production thus leading to formation of more wood ash waste. The study focuses on incorporation of wood ash in combination with ordinary Portland cement while using it for various structural works. A critical review study in sieve analysis, consistency, and water absorption, setting time and slump tests of wood ash added to OPC will produce significant results to emphasize the detailed study process. Uncontrolled burning of saw dust to form wood ash is used as a partial replacement of cement, thereby changing its physical and chemical properties. These properties are found somewhat similar to fly ash. The concrete mixes are replaced with the amorphous wood ash as an admixture of cement having grain size less than 75 microns in proportions of 5%, 10%, 15%, 20%, 25% and 30% by weight of cement. In this Study, a research work is conducted for determining the change in workability or consistency of concrete mix, compressive strength, split tensile strength, flexural strength, etc., along with review of some durability properties. Foundry Sand is used as fine aggregate to obtain efficient results.
机译:在纸浆和造纸厂,蒸汽发电厂和其他火力发电设施的锅炉中燃烧时,燃烧时会产生木灰作为残余物/废物。由于木材是能量的可再生资源和环境友好的材料,因此越来越需要使用废木材来生产能源,从而导致形成更多的木灰废物。该研究的重点是将木灰与普通波特兰水泥结合使用,同时将其用于各种结构工程。在筛分分析,稠度和吸水率,OPC中添加的木灰的凝结时间和坍落度测试方面进行的重要审查研究将产生重要结果,以强调详细的研究过程。锯末的无节制燃烧形成木灰被用作水泥的部分替代品,从而改变了其物理和化学性质。发现这些性质与粉煤灰有些类似。将混凝土混合物用无定形木灰代替,其作为水泥混合物,其具有小于75微米的粒度,按水泥重量的5%,10%,15%,20%,25%和30%的比例。在这项研究中,进行了一项研究工作,以确定混凝土混合物的可加工性或稠度,抗压强度,劈裂抗拉强度,抗弯强度等的变化,以及对某些耐久性能的评估。铸造砂被用作细骨料以获得有效的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号