MgO-ZrO2 powder (MZ30) containing 30 wt% MgO was prepared by simple precipitation method. Two other catalysts were obtained by loading MZ30 powder with 5 wt% SrO and CsO using incipient wetness impregnation method. The catalytic performance of these catalysts was evaluated for synthesis of 2-amino-2-chromene via one pot three components condensation of benzaldhyde with malononitrile and α-naphthol. Different techniques such as N2 physisorption, TGA-DTA, XRD, TEM, Hammet indicator method and CO2-TPD have been used to characterize the investigated catalysts. Reaction paameters such as reaction temperature, synthesis time and catalyst amount were studied to optimize the reaction conditions. The observed activity of these catalysts were correlated to their basicity and other surface parameters. Synthesis of 2-amino-2-chromene may involve moderate and strong basic sites of PKBH+ in the range ≥ 9.8 and ≤ 15.0. Base sites of PKBH+ are too weak to contribute in the synthesis processes.
机译:通过简单的沉淀法制备含有30重量%的MgO的MgO-ZrO 2粉末(MZ30)。使用初期湿润浸渍法通过向MZ30粉末中加入5 wt%的SrO和CsO来获得另外两种催化剂。通过一锅三组分苯甲醛与丙二腈和α-萘酚的缩合反应,评估了这些催化剂的催化性能,以合成2-氨基-2-色烯。已使用了不同的技术(例如氮气物理吸附,TGA-DTA,XRD,TEM,Hammet指示剂方法和CO2-TPD)来表征所研究的催化剂。研究了反应温度,合成时间和催化剂用量等反应参数,以优化反应条件。这些催化剂的观察到的活性与其碱性和其他表面参数相关。 2-氨基-2-色烯的合成可能涉及PKBH +的中度和强碱性位点,范围≥9.8和≤15.0。 PKBH +的碱基太弱,无法参与合成过程。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号