Refining of so-called opportunity crude oils with a high level of naphthenic acids and sulfur compounds has been increasing interest due to limited availability of light crude oils, however, considerable corrosive effects in the processing to high temperature on pipes and distillation towers mainly by the attack of naphthenic acids and sulfur compounds; sulfur compounds could be corrosive or can reduce the attack of naphthenic acids due to the formation of sulfides layers on the metal surface. In this work was evaluated the performance of deposits formed on the surface of carbon steel AISI SAE 1020 and 5% Cr-0.5% Mo steel exposed in crude oil fractions obtained from atmospheric distillation tower. For this, gravimetric tests were performed in dynamic autoclave using metal samples pre-treated in a crude oil fraction obtained from the atmospheric distillation tower of the Crude Distillation Unit (CDU) # 1 in order to form layers of sulfides on the surface of the two materials and subsequently to expose pre-treated and non-pretreated samples in two different crude oil fractions obtained from atmospheric distillation tower of Crude Distillation Unit (CDU) # 2. The evaluation showed that the samples pretreated decreased tendency to corrosion by naphthenic acids and sulfidation compared to untreated samples.
机译:由于轻质原油的供应有限,人们对利用环烷酸和硫化合物含量高的所谓机会原油进行精制的兴趣日益浓厚,但是,高温处理对管道和蒸馏塔的腐蚀作用很大,主要是因为环烷酸和硫化合物的侵蚀;由于在金属表面形成硫化物层,硫化合物可能具有腐蚀性或可以减少环烷酸的侵蚀。在这项工作中,评估了从常压蒸馏塔获得的原油馏分中暴露在碳钢AISI SAE 1020和5%Cr-0.5%Mo钢表面上形成的沉积物的性能。为此,在动态高压釜中使用从原油馏分(CDU)#1的常压蒸馏塔获得的原油馏分中经过预处理的金属样品进行了重量测试,以便在两者的表面上形成硫化物层。原料,然后将预处理和未经预处理的样品暴露在两个不同的原油馏分中,这些原油馏分从原油蒸馏塔(CDU)#2的常压蒸馏塔获得。评估表明,预处理的样品降低了环烷酸和硫化物的腐蚀趋势与未处理的样品相比。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号