This research assessed the performance of mortars in which recycled concrete aggregates (RCA) was a component. It replaced natural sand but kept the same particle size distribution. Three mortars were produced with replacement ratios of 20%, 50% and 100% as well as a reference mortar containing no recycled aggregate. The compressive and flexural strength, water absorption by capillarity, drying capacity and susceptibility to cracking of these mortars were analyzed first. Then, based on these results, the most satisfactory replacement ratio was chosen and the following properties were analyzed: water retentivity, shrinkage, adhesive strength, modulus of elasticity, and water vapor permeability. Somewhat surprisingly the best results in the first stage occurred for 20% and 100% replacement ratios, leading to a cautious choice of the 20% ratio for the second stage. Generally the mortar with 20% replacement ratio performed better than the reference mortar, except for adhesive strength and dimensional stability.
机译:这项研究评估了以再生混凝土骨料(RCA)为成分的砂浆的性能。它代替了天然沙子,但保持了相同的粒度分布。生产了三种砂浆,其替代率为20%,50%和100%,以及一种不含再生骨料的参考砂浆。首先分析了这些砂浆的抗压强度和抗折强度,毛细作用的吸水率,干燥能力和开裂敏感性。然后,基于这些结果,选择了最令人满意的置换率,并分析了以下性能:保水性,收缩率,粘合强度,弹性模量和水蒸气渗透性。出乎意料的是,第一阶段的最佳结果出现在20%和100%的替换率上,导致第二阶段谨慎选择20%的比率。通常,除了粘合强度和尺寸稳定性外,替代比为20%的砂浆的性能要优于参考砂浆。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号