Sources that can lead to deterioration of steam superheater tubes of a high pressure boiler were studied by a stress analysis, focused on internal pressure and temperature experienced by the material at real operating conditions. Loss of flame control, internal deposits and unexpected peak charge are factors that generate loads above the design limit of tube materials, which can be subjected to strain, buckling, cracks and finally rupture in service. To evaluate integrity and dependability of these components, the microstructure of selected samples along the superheater was studied by optical microscopy. Associated with this analysis, dimensional inspection, nondestructive testing, hardness measurement and deposit examination were made to determine the resultant material condition after twenty three years of operation.
机译:通过应力分析研究了可能导致高压锅炉蒸汽过热器管变质的源,重点是材料在实际操作条件下所经历的内部压力和温度。失去火焰控制,内部沉积物和意外的峰值电荷是导致超出管材设计极限的载荷的因素,这些载荷可能会承受应变,屈曲,破裂并最终在使用中破裂。为了评估这些组件的完整性和可靠性,通过光学显微镜研究了沿过热器选择的样品的微观结构。结合此分析,进行了二十三年的运行后,进行了尺寸检查,无损检测,硬度测量和沉积物检查,以确定最终的材料状态。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号