Effect of heat treatment on the mechanical strength, intergranular and exfoliation corrosion of 7075 aluminum alloy

机译:热处理对7075铝合金力学性能,晶间腐蚀和剥落腐蚀的影响

获取原文
           

摘要

In this study, the effects of heat treatments in the peak aged (T6), overaged (T73) and retrogression and reaging (RRA, retrogression at 200 ?°C for 10 min) on the microstructure, mechanical strength, exfoliation corrosion and intergranular corrosion of aluminum alloy 7075, has been investigated by optical microscope, scanning electron microscopy, tensile tests, ASTM G110 tests, ASTM G34 tests, polarization curve and electrochemical impedance spectroscopy (EIS). The results of intergranular corrosion tests (ASTM G110) and exfoliation corrosion tests (ASTM G34), applied to the three treatments defines an order of susceptibility to corrosion given by: T6 T73 RRA. The trends of the corrosion resistance were further confirmed by polarization curve and EIS test. The RRA heat treatment improved the intergranular-exfoliation corrosion resistance of aluminum alloy 7075 without sacrificing the mechanical strength compared to T6 temper. The effect of heat treatment on mechanical strength and corrosion resistance is explained based on the state of precipitation in the matrix and grain boundaries.
机译:在这项研究中,热处理对峰值时效(T6),过度时效(T73)以及回退和再老化(RRA,在200°C下回退10分钟)的影响对组织,机械强度,剥落腐蚀和晶间腐蚀已经通过光学显微镜,扫描电子显微镜,拉伸试验,ASTM G110试验,ASTM G34试验,极化曲线和电化学阻抗谱(EIS)对7075铝合金进行了研究。应用于三种处理的晶间腐蚀试验(ASTM G110)和剥落腐蚀试验(ASTM G34)的结果定义了对腐蚀的敏感性顺序,由下式给出:T6> T73> RRA。极化曲线和EIS测试进一步证实了耐蚀性的趋势。与T6回火相比,RRA热处理提高了7075铝合金的抗晶间剥落腐蚀性能,而没有牺牲机械强度。根据基体和晶界中的析出状态来说明热处理对机械强度和耐蚀性的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号