【24h】

Effects of plasma surface treatment on bending strength and modulus of elasticity of beech and poplar plywood

机译:等离子表面处理对榉木和杨木胶合板的弯曲强度和弹性模量的影响

获取原文
           

摘要

This is a study on the effect of plasma treatment with different gases and plasma intensity on the bending strength and modulus of elasticity of plywood manufactured from beech and poplar. Oxygen (O2) and ammonia (NH3) plasma were applied on the veneer sheets; two plasma intensities were applied on the veneers with 150 and 300 W in the plasma chamber during one minute. Phenol formaldehyde resin was applied on one surfaces of each veneer with approx. 160 g/m2. Bending strength and modulus of elasticity were determined according to EN 310.The effects of plasma surface treatment on chemical structure of the panels were determined with FTIR-ATR analysis. Bending strength of all tested panels slightly and partly increased without statistical significance when applying oxygen plasma. The effect of ammonia plasma treatment on bending strength and was determined by the wood species and the plasma intensity, and it was not uniform. Modulus of elasticity of the panels with oxygen plasma treatment showed in most cases improvement, whereas ammonia plasma pretreated veneers caused lower values compared to the control panels.
机译:这是对用不同气体和等离子体强度进行等离子体处理对山毛榉和杨木制成的胶合板的弯曲强度和弹性模量的影响的研究。将氧气(O2)和氨气(NH3)等离子体施加到饰面板上;一分钟内,在等离子室中分别在150和300 W的胶合板上施加了两个等离子强度。将苯酚甲醛树脂涂在每个贴面的一个表面上,约0.5mm。 160克/平方米。根据EN 310确定弯曲强度和弹性模量。通过FTIR-ATR分析确定等离子表面处理对面板化学结构的影响。当施加氧等离子体时,所有测试板的弯曲强度略有增加,但没有统计学意义。氨等离子体处理对弯曲强度的影响取决于木材种类和等离子体强度,并且不均匀。在大多数情况下,采用氧等离子体处理的面板的弹性模量显示有所改善,而经氨等离子体预处理的贴面与控制面板相比,其值较低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号