Abstract In the study, we successfully produced electrospun cellulose fibers crosslinked with β-CD. For electrospinning, cellulose was dissolve in 1-ethyl-3-methylimidazolium acetate and DMF was added to the prepared solution for better spinnability. The prepared cellulose fiber was immersed in the solution containing β-CD, crosslinking agent and sodium hypophosphite. In order to understand the effect of a crosslinking agent, two different types of the agents, BTCA (1,2,3,4-butanetetracarboxylic acid) and citric acid with various concentrations were used for cross-linking. The crosslinking degree was increased with the concentration of the crosslinking agents, for the both agents. The cross-linked web changed into membrane like morphology when the concentration of the cross-linking agent was higher than 5 wt%. The concentration of crosslinking agent also gave influence on the crystallinity, the thermal property and the antibacterial activity of fibers. Due to the cross-linking the crystallinity was decreased. The cross-linked fiber showed selective bacterial behavior according to the bacterial strain and the cross-linking agent.
机译:摘要在研究中,我们成功地生产了与β-CD交联的电纺纤维素纤维。为了进行静电纺丝,将纤维素溶解在乙酸1-乙基-3-甲基咪唑鎓中,并向制备的溶液中添加DMF,以提高纺丝性。将制得的纤维素纤维浸入含有β-CD,交联剂和次磷酸钠的溶液中。为了理解交联剂的作用,使用两种不同类型的交联剂BTCA(1,2,3,4-丁烷四羧酸)和柠檬酸以不同的浓度进行交联。对于两种试剂,交联度都随着交联剂浓度的增加而增加。当交联剂的浓度高于5wt%时,交联纤网变成膜状形态。交联剂的浓度还影响纤维的结晶度,热性能和抗菌活性。由于交联,结晶度降低。根据细菌菌株和交联剂,交联纤维表现出选择性的细菌行为。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号