摘要

Copper sulfide formation is one of the possible corrosion mechanisms involving the corrosive sulfur of copper. EDX scans of copper strip before and after immersing in aged transformer oils containing sulfur without copper passivator at 100°C for 3h indicated that copper sulfide was formed on the copper strip surface. The reclaimed oil by using kaolin clay reduced the sulfur content of all tested aged oils reducing the corrosion on copper strips in all samples investigated. In every case studied, the oil after reclamation by kaolin clay showed no sign at all of corrosive sulfur on the surface of copper strips. Nevertheless the atomic absorption analysis of copper ions in oil samples showed that the dissolution of copper was increased with increasing the sulfur content in the oil at different times of immersed copper strip in the oil.
机译:硫化铜的形成是涉及铜的腐蚀性硫的可能腐蚀机理之一。在没有铜钝化剂的情况下,将铜带浸入含硫的老化变压器油中并在100°C下浸泡3h之前和之后的EDX扫描表明,硫化铜形成在铜带表面。使用高岭土的再生油降低了所有测试过的老化油的硫含量,从而降低了所有研究样品中铜带的腐蚀。在每种研究的情况下,用高岭土回收的油在铜带表面上都没有显示出所有腐蚀性硫的迹象。然而,对油样中铜离子的原子吸收分析表明,在铜条浸入油中的不同时间,铜的溶解度随油中硫含量的增加而增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号