Visible light induced photocatalytic degradation of direct red 23 and direct brown 166 by InVO4-TiO2 nanocomposite

机译:可见光诱导的InVO4-TiO2纳米复合材料光催化降解直接红23和直接棕166

获取原文
           

摘要

The effect of various parameters (pH, irradiation time, nanophotocatalyst dosages and temperature) on photocatalytic degradation of Direct Red 23 (DR 23) and Direct Brown 166 (DB 166) using pure InVO4 and InVO4-TiO2 nanocomposite were investigated under visible light irradiation. InVO4 and InVO4-TiO2 were synthesized by hydrothermal and sol-gel/ hydrothermal treatment techniques, respectively and characterized by FT-IR spectroscopy, x-ray diffraction (XRD), diffuse reflectance UV–vis spectroscopy (DRS), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) images. Doping of TiO2 with InVO4 caused reduction in its band gap value with the resultant improvement in its visible light activity. The efficiency of nanocomposite on azo dyes degradation (pH 7.2, time: 30 min) reached high values (above 95%) under visible light, proving the remarkable photocatalytic activities of obtained composites. Moreover, the results indicated complete mineralization of DR 23 and DB 166 by InVO4- TiO2 under visible light for 300 min.
机译:在可见光照射下,研究了各种参数(pH,照射时间,纳米光催化剂的用量和温度)对使用纯InVO4和InVO4-TiO2纳米复合材料对直接红23(DR 23)和直接棕166(DB 166)的光催化降解的影响。 InVO4和InVO4-TiO2分别通过水热和溶胶-凝胶/水热处理技术合成,并通过FT-IR光谱,X射线衍射(XRD),漫反射紫外可见光谱(DRS),扫描电子显微镜(SEM)进行表征。 )和透射电子显微镜(TEM)图像。用InVO4掺杂TiO2导致其带隙值减小,从而改善了其可见光活性。在可见光下,纳米复合材料对偶氮染料的降解效率(pH 7.2,时间:30分钟)达到很高的值(95%以上),证明了所得复合材料具有显着的光催化活性。此外,结果表明InVO4-TiO2在可见光下300分钟使DR 23和DB 166完全矿化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号