The application of some semi-solid forming magnesium alloys is restricted due to their weak mechanical properties. To improve the mechanical properties, it is necessary to research the regularity and theory of semi-solid microstructure evolution of the alloy. In this study, microstructure evolution of ZA72 alloy during the partial remelting, and the effect of holding temperature and holding time on the semi-solid microstructure evolution of ZA72 magnesium alloy were investigated by means of OM, SEM and EDS analysis. The results indicate that the microstructure with small and spheroidal semi-solid particles which are available for thixo-forming can be obtained using proper heating parameters. After being isothermally treated at between 580 and 610 ℃ for 30 min, the equivalent size and shape factor of primary solid phase of ZA72 alloy decrease gradually, while the liquid volume fraction increases. When isothermally treated at 600 ℃ and held for different times from 15 to 60 min, with the increase of holding time, the equivalent size of primary particles decreases at first and then increases gradually; while the shape factor decreases gradually. The best heat treatment parameters in this experiment are to hold at 610 ℃ for 30 min. Compared with as-cast ZA72 alloy, the sizes of the eutectic phase and second α-Mg phase obtained in semi-solid state are smaller due to the higher solidification rate and the higher under-cooling degree than as-cast state. These decrease the fracture probability during tensile stress and improve the properties of the ZA72 alloy by semi-solid forming.
机译:一些半固态成形的镁合金由于其较弱的机械性能而受到限制。为了提高力学性能,有必要研究合金的半固态组织演变规律和理论。通过OM,SEM和EDS分析,研究了ZA72合金部分重熔过程中的组织演变,以及保温温度和保温时间对ZA72镁合金半固态组织演变的影响。结果表明,可以使用适当的加热参数获得具有小的和球形半固态颗粒的微结构,这些颗粒可以用于触变成形。 ZA72合金在580〜610℃等温热处理30分钟后,ZA72合金初生固相的当量尺寸和形状因子逐渐减小,液相体积分数增大。在600℃下等温保温15〜60min,随着保温时间的增加,一次颗粒的当量大小先减小后逐渐增大;而形状因子逐渐减小。本实验中最佳的热处理参数是在610℃下保持30分钟。与铸态ZA72合金相比,半铸态获得的共晶相和第二α-Mg相的尺寸较小,这是因为其凝固速率和过冷度都比铸态高。这些降低了拉伸应力时的断裂概率,并通过半固态成形改善了ZA72合金的性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号