This study investigates the strength properties of paper samples obtained from pulp blend of corn husk and kenaf bark. Soda pulping of kenaf bark and corn husk was carried out using 18% and 7% alkali respectively. Handmade paper sheets were produced from bleached pulp samples combined in ratios 50% - 50%, 75% - 25% and 25% - 75%. Using a universal testometric machine, strength properties of the papers such as modulus of elasticity, tensile index and tear index were assessed. Results showed that, paper sample from 100% kenaf bark has the highest tear index (20.72 mN.m2/g) and tensile index (7.79 Nm/g), while paper sample from mixture of Kenaf bark and Corn husk (75% - 25%) possess highest modulus of elasticity (42.05 N/mm2). Lowest tensile index (2.77 Nm/g) and modulus of elasticity (12.42 N/mm2) values were observed for paper sample from 100% corn husk. Depending on targeted end use, papers of differing strength properties can be obtained from the combination of kenaf bark and corn husk.
机译:这项研究调查了从玉米壳和洋麻树皮的纸浆混合物获得的纸样品的强度特性。洋麻树皮和玉米皮的苏打浆分别使用18%和7%的碱进行制浆。由漂白的纸浆样品以比例为50%-50%,75%-25%和25%-75%的比例生产手工纸片。使用通用的测试机,评估纸的强度特性,例如弹性模量,拉伸指数和撕裂指数。结果表明,从100%的洋麻树皮中提取的纸样具有最高的撕裂指数(20.72 mN.m2 / g)和拉伸指数(7.79 Nm / g),而从洋麻的树皮和玉米皮的混合物中提取的纸样(75% -25%)具有最高的弹性模量(42.05 N / mm2)。从100%的玉米壳中观察到的纸张样品的最低拉伸指数(2.77 Nm / g)和弹性模量(12.42 N / mm2)值。根据目标最终用途,可以从洋麻树皮和玉米皮的组合中获得具有不同强度特性的纸张。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号