Sludge dewatering was an important part of sludge treatment and disposal. Building a dewatering skeleton played a vital role in sludge dewatering. Experimental study on municipal sludge dewatering capacity was conducted by using quicklime and slag. Research indicated that sludge with 83% moisture content was conducive to establish the skeleton. Slag with large, small, or even particle diameters were disadvantageous to the skeleton formation, the effective combination range for the particle diameter was from 0.075 to 0.85 mm. When the sludge with 83% moisture content is added with 15% quicklime, it can reach the maximum dewatering rate and meet the health and epidemic-prevention safety index. The moisture content was lower than 60% with the following conditions: 83% moisture content of sludge, 15% quicklime, >= 80% slag, and 3,000-4,200 separation factors which satisfied various engineering applications such as landfills, ecological slope protection, and landscaping.
机译:污泥脱水是污泥处理和处置的重要组成部分。建立脱水骨架在污泥脱水中起着至关重要的作用。利用生石灰和矿渣进行城市污泥脱水能力的实验研究。研究表明,含水量为83%的污泥有助于建立骨架。具有大,小或什至粒径的炉渣不利于骨架的形成,粒径的有效组合范围为0.075至0.85mm。当添加水分含量为83%的污泥和15%的生石灰时,可以达到最大脱水率并达到健康和防疫安全指标。在以下条件下水分含量低于60%:污泥水分含量83%,生石灰15%,矿渣> = 80%和3,000-4,200的分离系数,可满足各种工程应用,如垃圾填埋场,生态护坡和美化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号