Reduced activation ferritic/martensitic steel F82H samples with tritium permeation barriers were annealed in contact with ceramic breeder pebbles at 550 degrees C and 700 degrees C for up to 32 days under purge gas. Cr2O3-formed F82H rapidly reacted to form three layers at 550 degrees C, and pure Fe projections grew with annealing time. Diffusion kinetics of O and Li were well fitted with Fick's first law of diffusion. Er2O3 coatings did not react with the pebbles, but deteriorated by oxygen diffusion through the coatings. The impurity concentrations in the system and the coating thickness affect the coating compatibility in solid breeder blanket environments.
机译:减少的活化铁素体/马氏体钢F82H样品具有氚渗透屏障的样品在550℃和700摄氏度下与陶瓷种植卵石接触,在吹扫气体下长达32天。 CR2O3形成的F82H快速反应以在550℃下形成三层,纯Fe突起随着退火时间而增长。 O和Li的扩散动力学与Fick的第一款扩散定律合作。 ER2O3涂层与鹅卵石没有反应,但通过涂层的氧气扩散劣化。系统中的杂质浓度和涂层厚度影响固体种类毯子环境中的涂层相容性。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号