Tribocorrosion behaviour of aluminium bronze in 3.5 wt.% NaCl solution

机译:铝青铜在3.5 wt。%NaCl溶液中的摩擦腐蚀行为

获取原文
获取原文并翻译 | 示例

摘要

Tribocorrosion behaviour of aluminium bronze CuAl10Fe5Ni5 in 3.5 wt.% NaCl solution was investigated in a pin-on-disc facility containing an electrochemical cell. Oxidising capacity and contact pressure to alumina counterbody were varied. Pure corrosion occurred as selective dissolution of a phase included in the eutectoid structure. Contact to counterbody introduced plastic deformation, extrusion of the material and abrasive wear. Wear-corrosion interactions varied between the two contact pressures, with lower material losses appearing at the higher pressure. The significant acceleration of material degradation by the interactions was not clearly reflected to kinetics or thermodynamics of corrosion. These results are presented and discussed here.
机译:在包含电化学电池的针对盘设备中研究了铝青铜CuAl10Fe5Ni5在3.5 wt%NaCl溶液中的摩擦腐蚀行为。氧化能力和对氧化铝配体的接触压力是变化的。由于共析结构中所含相的选择性溶解而发生纯腐蚀。与对方的接触导致塑性变形,材料挤压和磨料磨损。磨损与腐蚀的相互作用在两个接触压力之间变化,较高的压力下出现的材料损失较小。相互作用引起的材料降解的显着加速没有清楚地反映到腐蚀的动力学或热力学上。这些结果在此处介绍和讨论。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号