This study presents laboratory evaluation integrated with field performance to examine two widely used warm-mix asphalt (WMA) approaches—foaming and emulsion technology. For a more realistic evaluation of the WMA approaches, trial pavement sections of the WMA mixtures and their counterpart hot-mix asphalt (HMA) mixtures were implemented in Antelope County, Nebraska. Field-mixed loose mixtures collected at the time of paving were transported to the laboratories to conduct various experimental evaluations of the individual mixtures. Among the laboratory tests, three (two conventional and one newly attempted) were performed to characterize moisture damage potential which is the primary focus of this study. From the laboratory test results, WMA mixtures showed greater susceptibility to moisture conditioning than the HMA mixtures, and this trend was identical from multiple moisture damage parameters including the strength ratio and the critical fracture energy ratio. Early-stage field performance data collected for three years after placement presented satisfactory rutting-cracking performance from both the WMA and HMA sections, which generally agrees with laboratory evaluations. Although the field performance data indicated that both the WMA and HMA show similar good performance, careful observation of field performance over a period of years is necessary since moisture damage can be accelerated after rutting or cracking as a later-stage pavement distress.
机译:这项研究提出了结合现场性能的实验室评估,以研究两种广泛使用的温拌沥青(WMA)方法-发泡和乳液技术。为了更真实地评估WMA方法,在内布拉斯加州的羚羊县实施了WMA混合物及其对应的热拌沥青(HMA)混合物的试验路面部分。摊铺时收集的现场混合的松散混合物被运送到实验室,对各个混合物进行各种实验评估。在实验室测试中,进行了三项测试(两项常规测试,另一项是新尝试),以表征潜在的湿气损害,这是本研究的主要重点。从实验室测试结果来看,WMA混合物比HMA混合物对水分调节的敏感性更高,并且这种趋势在多个水分破坏参数(包括强度比和临界断裂能比)中是相同的。放置后三年收集的早期现场性能数据显示,WMA和HMA部分的车辙开裂性能令人满意,这与实验室评估基本一致。尽管现场性能数据表明WMA和HMA都表现出相似的良好性能,但由于在后车辙或开裂后会加速湿气损坏,这是后期路面问题的原因,因此必须仔细观察多年的现场性能。

著录项

  • 来源
    《Construction and Building Materials 》 |2012年第2012期| p.204-211| 共8页
  • 作者单位

    Department of Civil Engineering, 224 Engineering Building, Kyung Hee University, Yongin-si, Gyeonggi-do 446-701, South Korea;

    Department of Civil Engineering, 362 Whittier Research Center, University of Nebraska, Lincoln, NE 68583, USA;

    Department of Civil Engineering, 362H Whittier Research Center, University of Nebraska, Lincoln, NE 68583, USA;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    warm-mix asphalt; moisture damage; field performance; laboratory evaluation;

    机译:温拌沥青;湿气损害现场表现;实验室评估;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号