The aim of study is to evaluate rutting with Marshall Quotient (MQ) and repeated creep (RCT). Three hydrated lime (HL) mixtures were evaluated and compared with control mixtures (CMs) for conditioned samples (CSs). Filler was reduced and HL was substituted at 2%, 4% and 6%. Damage system (ECS) based on moisture was applied. For rutting with MQapproach also some mixtures were produced including SBS and HL Modified and synergistic (SBS and HL) mixtures were interrogated. An observed damage level was exposed with the selected ECS. RCT was quite effective at different HL ratios for HL efficiency for dense gradation. HL was found beneficial due to moisture. Increasing of HL from 2% to 6% deformation resistance increased. Tertiary deformation was not revealed at 64,730 pulses for CM and HL ones. Expected results were obtained with the RCT for both HL mixtures and also SBS. MQ is not a good indicator of the deformation resistance because of the larger intervals between CM and others.
机译:研究的目的是评估马歇尔商数(MQ)和重复蠕变(RCT)的车辙。评估了三种熟石灰(HL)混合物,并将其与对照混合物(CMs)进行了条件样品(CSs)的比较。减少填充物,并以2%,4%和6%的HL取代。应用了基于水分的破坏系统(ECS)。为了使用MQapproach进行车辙,还生成了一些混合物,包括SBS和HL Modified,并询问了协同(SBS和HL)混合物。选择的ECS暴露了观察到的损坏程度。在不同的HL比率下,RCT对于密集层次的HL效率非常有效。由于水分,HL被认为是有益的。 HL的抗变形性从2%增加到6%。 CM和HL脉冲在64,730个脉冲时没有发现三次变形。使用RCT对HL混合物和SBS均获得了预期的结果。 MQ并不是变形抗力的良好指标,因为CM与其他物体之间的间隔较大。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号