Limited field data are available from reinforced concrete specimens exposed to environmental conditions and subjected to severe deterioration by Alkali Silica Reaction (ASR) and/or Delayed Ettringite Formation (DEF). A large-scale reinforced concrete specimen is subject to ASR/DEF deterioration for five years. Strain measurements indicate that both transverse and longitudinal reinforcement yield within six to twelve months of field exposure. Recorded surface strains compare well with the internal steel and concrete strains. Transverse expansion strains markedly exceed longitudinal expansion strains. Although ASR/DEF deterioration may cause severe surface cracking and possible reinforcement corrosion in the long-term, its effect on the structure's load carrying capacity remains unknown at this time. (C) 2016 Elsevier Ltd. All rights reserved.
机译:有限的现场数据可从暴露于环境条件并受到碱二氧化硅反应(ASR)和/或延迟钙矾石形成(DEF)严重破坏的钢筋混凝土样品中获得。大型钢筋混凝土标本会经受五年的ASR / DEF劣化。应变测量表明,在野外暴露的6到12个月内,横向和纵向钢筋均屈服。记录的表面应变与内部钢和混凝土应变比较好。横向膨胀应变明显超过纵向膨胀应变。尽管从长期来看,ASR / DEF的劣化可能会导致严重的表面开裂和可能的钢筋腐蚀,但目前尚不清楚其对结构的承载能力的影响。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号