A simple test method in order to assess the effect of mineral fillers on bitumen ageing

机译:一种简单的测试方法,用于评估矿物填料对沥青老化的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Bitumen has been known to be prone to chemical ageing from the very beginning of its modern use in road construction. It is now well accepted that this results in chemical changes illustrated in particular by an increase in asphaltenes content and in the quantity of functional groups such as sulfoxides and carbonyls. The rheological consequences are a global hardening and embrittlement. However, the role of other potential ingredients of asphalt mixtures on bitumen oxidation kinetics remain poorly documented. If hydrated lime has been observed to reduce ageing for more than 40 years, the role of other mineral fillers is not so clear. Part of the problem comes from the difficulty to use the current standard ageing procedures for bitumen when it comes to mastics (blends of bitumen and filler). The viscosity increase due to the presence of filler decreases the severity of the ageing process in rotating methods such as the celebrated Rolling Thin Film Oven Test (RTFOT). Therefore, we developed a simple procedure based on the existing Pressure Aging Vessel (PAV) and on published equivalence between RTFOT and PAV. This makes it possible to easily quantify the effect of mineral fillers through an increase in ring and ball softening temperature, independent of the viscosity increase due to the filler. Using this method, it is shown that hydrated lime slows down bitumen ageing more than other less active fillers such as hydraulic lime or Portland cement, and that mineral fillers from crushed limestone or granitic aggregate have no effect on bitumen ageing. (C) 2016 Elsevier Ltd. All rights reserved.
机译:从沥青在道路建设中的现代使用之初就已知它易于发生化学老化。现在已经众所周知,这导致化学变化,特别是通过增加沥青质含量和增加官能团例如亚砜和羰基的量来说明。流变学后果是整体硬化和脆化。但是,沥青混合料中其他潜在成分对沥青氧化动力学的作用仍然文献很少。如果观察到熟石灰可以减少老化超过40年,那么其他矿物填料的作用还不是很清楚。问题的部分原因是涉及到胶泥(沥青和填充料混合物)时,难以使用当前标准的沥青老化程序。由于存在填料而导致的粘度增加降低了旋转方法(例如著名的滚动薄膜烤箱测试(RTFOT))中时效过程的严重性。因此,我们基于现有的压力老化容器(PAV)以及已发布的RTFOT和PAV之间的等效性,开发了一种简单的程序。这使得可以通过增加环和球的软化温度来容易地量化矿物填料的效果,而与由于填料引起的粘度增加无关。使用这种方法表明,熟石灰比水硬性石灰或硅酸盐水泥等其他活性较低的填料更能减缓沥青的老化,碎石灰石或花岗岩骨料的矿物填料对沥青的老化没有影响。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

  • 来源
    《Construction and Building Materials》 |2016年第1期|182-189|共8页
  • 作者单位

    Tour W, Lhoist, 102 Terrasse Boieldieu, F-92085 Paris, France;

    Ctr Formacao Prof Ind Construcao Civil & Obras Pu, Rua Espinhosa, P-4475699 Avioso S Pedro, Maia, Portugal;

    Ciesm Intevia, Parque Empresarial Barajas Pk,C San Severo 18, Madrid 28042, Spain;

    Ciesm Intevia, Parque Empresarial Barajas Pk,C San Severo 18, Madrid 28042, Spain;

    Ciesm Intevia, Parque Empresarial Barajas Pk,C San Severo 18, Madrid 28042, Spain;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Asphalt; Bitumen; Ageing; Oxidation; Test method; Mineral filler; Hydrated lime; Cement;

    机译:沥青;老化;氧化;测试方法;矿物填料;熟石灰;水泥;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号