In order to investigate the effect of aggregates on the concrete sulfuric acid resistance, accelerated corrosion experiments were conducted with four types of concretes composed of coarse and fine aggregates with two different chemical compositions. All the concretes with the same water/cement ratio of 0.45, and the pH value was kept in the range of 0.93-0.97. With continuous monitoring of each concrete specimen, corrosion depth, mass loss, and dynamic modulus elasticity loss were calculated. The results showed that the dynamic modulus of elasticity loss can be regard as an acceptable indicator for evaluating the resistance of concrete to sulfuric acid attack as well as corrosion depth and mass loss. A regression model proposed in this paper could provide good predictions. Concrete with marble aggregates rich in calcium carbonate have better performances in sulfuric acid solution than that with inert aggregates. Effect of fine aggregate on concrete sulfuric acid corrosion rate is more significant than coarse aggregate in the term of corrosion depth, mass loss, and dynamic modulus of elasticity loss. (C) 2016 Elsevier Ltd. All rights reserved.
机译:为了研究骨料对混凝土耐硫酸性的影响,对由两种具有不同化学成分的粗骨料和细骨料组成的四种类型的混凝土进行了加速腐蚀实验。水灰比相同的所有混凝土为0.45,pH值保持在0.93-0.97范围内。通过连续监测每个混凝土试样,计算出腐蚀深度,质量损失和动态模量弹性损失。结果表明,动态弹性模量损失可以作为评估混凝土抗硫酸侵蚀性以及腐蚀深度和质量损失的可接受指标。本文提出的回归模型可以提供良好的预测。富含碳酸钙的大理石集料的混凝土在硫酸溶液中的性能要优于惰性集料的混凝土。就腐蚀深度,质量损失和动态弹性模量损失而言,细骨料对混凝土硫酸腐蚀速率的影响比粗骨料大。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号