Fatigue performance of bituminous mixtures made with recycled concrete aggregates and waste tire rubber

机译:再生混凝土骨料和废轮胎橡胶制成的沥青混合物的疲劳性能

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Fatigue cracking is one of the main hot-mix asphalt (HMA) failure modes. The current laboratory investigation analyses the fatigue performance of HMA made with recycled concrete aggregates (RCA). An HMA type AC 22 bin S made with 0%, 35% and 42% of RCA was tested in the indirect tensile fatigue test (ITFT) device. Three constant stress levels, ranging from 150 kPa to 350 kPa were used. Mixtures were manufactured at the optimum bitumen content using two types of bitumen: a B35/50 penetration grade bitumen and a 10% waste tire rubber modified bitumen, BC35/50. This investigation demonstrates the beneficial effect on fatigue life of the incorporation of RCA. Additionally, the use of crumb rubber could lead to RCA bituminous mixtures with higher fatigue life in medium traffic roads. (C) 2017 Elsevier Ltd. All rights reserved.
机译:疲劳开裂是主要的热混合沥青(HMA)破坏模式之一。当前的实验室调查分析了由再生混凝土骨料(RCA)制成的HMA的疲劳性能。在间接拉伸疲劳测试(ITFT)设备中测试了由0%,35%和42%的RCA制成的HMA型AC 22 binS。使用了三个恒定应力水平,范围从150 kPa到350 kPa。使用两种类型的沥青以最佳的沥青含量生产混合物:B35 / 50渗透级沥青和10%废轮胎橡胶改性沥青BC35 / 50。这项研究证明了加入RCA对疲劳寿命的有益影响。另外,使用碎橡胶可能会导致RCA沥青混合物在中等交通道路上具有更高的疲劳寿命。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号