Alkaline activated concretes based on a mixture of fly ash (FA) and blast furnace slag (GBFS), as well as FA and Portland cement (OPC), both at a ratio of 80:20, were exposed to temperatures between 25 degrees C and 1100 degrees C. Then, the physicochemical and mechanical changes were evaluated. The results indicate that the activated concretes have better performance than the reference ones (100% OPC). At temperatures of 1100 degrees C, the residual strengths of the FA/GBFS and FA/OPC concretes are 15 and 5.5 MPa, respectively, unlike the OPC concrete that lost 100% of its strength. At temperatures above 900 degrees C, the activated matrix densified, and the crystalline phases, such as sodalite, nepheline, albite and akermanite, are identified. (C) 2017 Elsevier Ltd. All rights reserved.
机译:将粉煤灰(FA)和高炉矿渣(GBFS),FA和波特兰水泥(OPC)的比例为80:20的碱性活化混凝土暴露在25摄氏度至25摄氏度之间的温度下。 1100℃。然后,评估其物理化学和机械变化。结果表明,活化混凝土具有比参考混凝土(100%OPC)更好的性能。在1100摄氏度的温度下,FA / GBFS和FA / OPC混凝土的残余强度分别为15和5.5 MPa,这与OPC混凝土失去100%的强度不同。在高于900摄氏度的温度下,活化的基质致密化,并鉴定出结晶相,例如方钠石,霞石,钠长石和钙钛矿。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号