Autogenous shrinkage of slag-fly ash blends activated with hybrid sodium silicate and sodium sulfate at different curing temperatures

机译:用杂交硅酸钠和硫酸钠在不同固化温度下激活炉渣粉煤灰混合物的自生收缩

获取原文
获取原文并翻译 | 示例
           

摘要

This study investigates the effect of sodium sulfate concentration and curing temperature (20 degrees C and 40 degrees C) on the autogenous shrinkage of hybrid sodium silicate and sodium sulfate activated slag/fly ash systems (AASF). Regardless of the curing temperature, the main reaction products formed are C-A-S-H gels, and no formation of N-A-S-H type gels is observed in the studied AASF systems. Due to increase in rate of reaction and refinement of the pore structure, the autogenous shrinkage increased with increasing sodium sulfate concentration. At a high curing temperature (40 degrees C), the decrease in rate of autogenous shrinkage with time is primarily attributed to the suppression of the self-desiccation process due to decrease in reaction rate, and formation of a matrix with high elastic modulus or restrain effect at early ages. Furthermore, the increase in crystallinity of C-A-S-H gels is also responsible for a lower autogenous shrinkage in samples cured at 40 degrees C. Ettringite does not form to compensate the autogenous shrinkage at early hours. (C) 2020 Elsevier Ltd. All rights reserved.
机译:本研究研究了硫酸钠浓度和固化温度(20℃和40℃)对杂交硅酸钠和硫酸钠活性炉渣/飞灰系统(AASF)的自体收缩的影响。无论固化温度如何,所形成的主要反应产物是C-A-S-H凝胶,并且在研究的AASF系统中没有观察到N-A-S-H型凝胶的形成。由于孔隙结构的反应速率和细化的增加,随着硫酸钠浓度的增加而增加,自生收缩增加。在高固化温度(40摄氏度)中,随着时间的时间和时间的自生收缩率的降低主要归因于由于反应速率降低而抑制自灭过程,以及具有高弹性模量或抑制的基质的形成早期的效果。此外,C-A-S-H凝胶的结晶度的增加也是在40摄氏度固化的样品中的较低自体收缩的原因。Ettringite不形成以补偿初期的自生收缩。 (c)2020 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号