A new experimental methodology for studying ASR expansions at the level of a single aggregate-cementitious matrix interface is proposed. For this methodology, small sandwich-like specimens, with cement paste or mortar on top and bottom of a disc of soda-lime (SL) glass in the middle, are used. These specimens are placed in airtight containers with an alkaline solution and heated in an oven at 60 degrees C. In these conditions, ASR products are formed rapidly at the interface of the disc and the cementitious matrix, inducing length changes in the specimen which are measured regularly. The morphology and composition of the ASR products are studied by means of SEM/EDS analyses. This inexpensive and very easy to replicate methodology may provide valuable information about the ASR expansion mechanisms. The specimens developed expansions of about 30 mu m before the SL glass got detached from the cement paste matrix. SEM/EDS analyses of the reaction products formed in between the SL glass and the cement paste matrix indicate calcium-to-silica molar ratios ranging between 1.0 and 1.5. Finally, based on the experimental results presented in this paper, as well as on other experimental and theoretical results found in the literature, a reaction-expansion mechanism for ASR in SL glass concrete is proposed. (C) 2019 Elsevier Ltd. All rights reserved.
机译:提出了一种新的实验方法,用于研究单个骨料-胶结矩阵界面水平的ASR扩展。对于此方法,使用小的三明治状标本,中间是一盘钠钙玻璃(SL)的顶部和底部带有水泥浆或砂浆。将这些样品放置在带有碱性溶液的密闭容器中,并在60°C的烤箱中加热。在这些条件下,ASR产物会在圆盘和水泥基体的界面处迅速形成,从而导致所测样品的长度变化经常。通过SEM / EDS分析研究了ASR产物的形态和组成。这种廉价且非常易于复制的方法可以提供有关ASR扩展机制的有价值的信息。在SL玻璃从水泥浆基质中分离出来之前,样品出现了约30微米的膨胀。在SL玻璃和水泥浆基质之间形成的反应产物的SEM / EDS分析表明,钙硅比为1.0至1.5。最后,根据本文提出的实验结果以及文献中发现的其他实验和理论结果,提出了SL玻璃混凝土中ASR的反应-扩展机理。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号