Compared with flat laminates, curved composite laminates are more susceptible to wrinkle defects which must be considered in the design and structural integrity assessment. Combined experimental testing and numerical simulations were carried out in this paper to investigate the influence of wrinkles on the failure behavior of L shaped laminates. Special lay-up and forming processes were used to generate the pre-defined wrinkle profiles, and mechanical test together with the DIC measurement were carried out to illustrate the impact of wrinkles. Numerical modelling with progressive failure analysis approach was developed to simulate the failure process and the influence of the wrinkles. It is revealed that wrinkles triggered premature delamination and alter the propagation process by inducing damages near wrinkle plies. A significant strength reduction of about 30-40% was observed for the specimen containing wrinkles by both the numerical simulation and experimental results. Failure mechanism analysis revealed that the influence of wrinkles on the failure behavior was attributed to local stress concentrations around the wrinkles. The geometrical features such as amplitude and locations of the wrinkles are important factors to be evaluated for engineering application of curved composite structures.
机译:与平板层压板相比,弯曲的复合层压板更容易受到皱纹缺陷,必须考虑在设计和结构完整性评估中。本文进行了组合的实验测试和数值模拟,以研究皱纹对L形层压板的失效行为的影响。使用特殊的铺设和形成过程来产生预定义的褶皱型材,并进行与DIC测量的机械测试以说明皱纹的影响。开发了具有渐进式故障分析方法的数值模拟,以模拟故障过程和皱纹的影响。据透露,皱纹触发过早分层并通过诱导皱纹层附近的损坏来改变传播过程。对于含有数值模拟和实验结果的样品,观察到含有皱纹的试样的显着强度降低。失败机制分析表明,皱纹对破坏行为的影响归因于皱纹周围的局部应力浓度。诸如皱纹的幅度和位置的几何特征是用于工程应用弯曲复合结构的重要因素。

著录项

  • 来源
    《Composite Structures》 |2021年第4期|113541.1-113541.14|共14页
  • 作者单位

    Adv Energy Sci & Technol Guangdong Lab Foshan Xianhu Lab Foshan 528000 Peoples R China|Wuhan Univ Technol Hubei Key Lab Theory & Applicat Adv Mat Mech Wuhan 430070 Peoples R China;

    Adv Energy Sci & Technol Guangdong Lab Foshan Xianhu Lab Foshan 528000 Peoples R China|Wuhan Univ Technol State Key Lab Adv Technol Mat Synth & Proc Wuhan 430070 Peoples R China;

    Adv Energy Sci & Technol Guangdong Lab Foshan Xianhu Lab Foshan 528000 Peoples R China|Wuhan Univ Technol State Key Lab Adv Technol Mat Synth & Proc Wuhan 430070 Peoples R China;

    Adv Energy Sci & Technol Guangdong Lab Foshan Xianhu Lab Foshan 528000 Peoples R China|Wuhan Univ Technol Hubei Key Lab Theory & Applicat Adv Mat Mech Wuhan 430070 Peoples R China|Wuhan Univ Technol State Key Lab Adv Technol Mat Synth & Proc Wuhan 430070 Peoples R China|Univ Bristol Dept Mech Engn Bristol BS8 1TR Avon England;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Curved laminates; Manufacturing defects; Wrinkles; Progressive failure;

    机译:弯曲的层压板;制造缺陷;皱纹;逐步失败;
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号