During heat transfer from metal to solution, local metal activation occurs more readily within a crevice than under isothermal conditions, i.e., both for metal open surface temperature and also for crevice bottom temperature. Metal within a crevice is activated more readily the higher the heat flow density. Disruption of passivity is more likely to occur in the form of a corrosion spot close to a crevice bottom.
机译:在从金属到溶液的热传递过程中,缝隙中的局部金属活化比等温条件下更容易发生,即对于金属开放表面温度和缝隙底部温度而言。缝隙中的金属越容易被激活,热流密度越高。钝化的破坏更可能以接近缝隙底部的腐蚀点的形式发生。