Eight-year wear analysis in Longevity highly cross-linked polyethylene liners comparing 26- and 32-mm heads

机译:Longevity高交联聚乙烯衬里的八年磨损分析,比较26毫米和32毫米的头部

获取原文
获取原文并翻译 | 示例
           

摘要

Introduction Although wear reduction of highly cross-linked polyethylene has been demonstrated to be independent of femoral head diameter in some simulation studies, the clinical effects of femoral head diameter on wear of highly cross-linked polyethylene sockets remain unclear. We compared the in vivo wear of Longevity highly cross-linked polyethylene liners at 8-year follow-up using 26- or 32-mm cobalt-chromium heads.
机译:引言尽管在一些模拟研究中已证明,减少高交联聚乙烯的磨损与股骨头直径无关,但对于高交联聚乙烯窝的磨损,股骨头直径的临床影响尚不清楚。我们比较了使用26毫米或32毫米钴铬合金头在8年的随访中Longevity高交联聚乙烯衬垫的体内磨损情况。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号