Thermal osteonecrosis and bone drilling parameters revisited

机译:热骨坏死和钻探参数重新

获取原文
获取原文并翻译 | 示例

摘要

During the drilling of the bone, the temperature could increase above 47°C and cause irreversible osteonecrosis. The result is weakened contact of implants with bone and possible loss of rigid fixation. The aim of this study was to find an optimal condition where the increase in bone temperature during bone drilling process would be minimal.
机译:在骨骼钻孔过程中,温度可能会升高到47°C以上,并导致不可逆的骨坏死。结果是削弱了植入物与骨骼的接触,并可能失去刚性固定。这项研究的目的是找到一个最佳条件,使骨骼钻孔过程中骨骼温度的升高降至最小。

著录项

  • 来源
    《Archives of Orthopaedic and Trauma Surgery 》 |2008年第1期| 71-77| 共7页
  • 作者单位

    Department of Surgery University Hospital Center Zagreb Kišpatićeva 12 10000 Zagreb Croatia;

    Department of Surgery University Hospital Center Zagreb Kišpatićeva 12 10000 Zagreb Croatia;

    Faculty of Mechanical Engineering and Naval Architecture Department of Technology Chair of Machine Tools Zagreb Croatia;

    Faculty of Mechanical Engineering and Naval Architecture Department of Technology Chair of Machine Tools Zagreb Croatia;

    Faculty of Chemical Engineering and Technology Department of Measurement and Process Control Zagreb Croatia;

    Department of Surgery University Hospital Center Zagreb Kišpatićeva 12 10000 Zagreb Croatia;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Thermal osteonecrosis; Bone drilling;

    机译:热坏死;骨钻;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号