首页> 外文期刊>Applied Surface Science >Surface modification of calcium fluoro and hydroxyapatite by 1-octylphosphonic dichloride
【24h】

Surface modification of calcium fluoro and hydroxyapatite by 1-octylphosphonic dichloride

机译:1-辛基膦酰二氯对氟钙和羟磷灰石的表面改性

获取原文
获取原文并翻译 | 示例
       

摘要

The reactivity of the surface of calcium hydroxyapatite (CaHAp) and fluorapatite (CaFAp) was tested and compared by grafting the 1-octylphosphonic dichloride (C_8H_(17)OPCl_2) using a molar ratio x=2 or 4, x- n(organic)(apatite). Successful synthesis was confirmed by different characterisation techniques such as X-ray powder diffraction patterns, IR spectroscopy, MAS-NMR (~1H and ~(31)P) and chemical analysis.The difference between their specific surface area (SSA: 57.46 for HAp and 12.09 m~2/g for FAp), the percentage of carbon measured after treatment with (C_8H_(17)OPCl_2) and the intensities of IR bands attributed to the grafted moiety suggests that the surface of hydroxyapatite is more reactive than that of fluorapatite. The ~(31)P CP-MAS-NMR spectra of treated fluorapatite show a significant change in isotropic signal due to the protonation and deprotonation of superficial phosphate group. This can be explained by the difference in the nature of inorganic material.
机译:通过使用摩尔比x = 2或4,x-n(有机)接枝1-辛基膦酰二氯(C_8H_(17)OPCl_2)测试并比较了羟基磷灰石钙(CaHAp)和氟磷灰石(CaFAp)表面的反应性/ n(磷灰石)。 X射线粉末衍射图谱,IR光谱,MAS-NMR(〜1H和〜(31)P)和化学分析等不同的表征技术证实合成成功,其比表面积之差(SSp:HAp为57.46) (对于FAp为12.09 m〜2 / g),用(C_8H_(17)OPCl_2)处理后测得的碳百分比以及归因于接枝部分的IR带强度表明,羟基磷灰石的表面比氟磷灰石的表面更具活性。经处理的氟磷灰石的〜(31)P CP-MAS-NMR光谱显示,由于表面磷酸基团的质子化和去质子化,各向同性信号发生了显着变化。这可以通过无机材料的性质差异来解释。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号