首页> 外文期刊>Applied clay science >Calcined tetrabutylammonium kaolinite and montmorillonite and adsorption of Fe(II), Co(II) and Ni(II) from solution
【24h】

Calcined tetrabutylammonium kaolinite and montmorillonite and adsorption of Fe(II), Co(II) and Ni(II) from solution

机译:煅烧的四丁基铵高岭石和蒙脱石以及溶液中对Fe(II),Co(II)和Ni(II)的吸附

获取原文
获取原文并翻译 | 示例
       

摘要

Kaolinite and montmorillonite were modified with tetrabutylammonium (TBA) bromide, followed by calcination. The structural changes were monitored with XRD, FTIR, surface area and cation exchange capacity measurements. The modified clay minerals were used for adsorption of Fe(III), Co(II) and Ni(II) ions from aqueous solution under different conditions of pH, time and temperature. The uptake of the metal ions took place by a second order kinetics. The modified montmorillonite had a higher adsorption capacity than the corresponding kaolinite. The Langmuir monolayer capacities for the modified kaolinite and montmorillonite were Fe(III): 9.3 mg g~(-1) and 22.6mg g~(-1); Co(II): 9.0 mg g~(-1) and 22.3 mg g~(-1), and Ni(II): 8.4 mg g~(-1) and 19.7 mg g~(-1). The modified kaolinite interacted with Co(II) in an endothermic manner, but all the other interactions were exothermic. The decrease of the Gibbs energy in all the cases indicated spontaneous adsorption.
机译:高岭石和蒙脱石用四丁基溴化铵(TBA)改性,然后煅烧。用XRD,FTIR,表面积和阳离子交换容量测量监测结构变化。改性粘土矿物用于在不同的pH,时间和温度条件下从水溶液中吸附Fe(III),Co(II)和Ni(II)离子。金属离子的吸收是通过二级动力学发生的。改性的蒙脱石比相应的高岭石具有更高的吸附能力。改性高岭石和蒙脱石的Langmuir单层容量为Fe(III):9.3 mg g〜(-1)和22.6mg g〜(-1); Co(II):9.0mg g·(-1)和22.3mg g·(-1),Ni(II):8.4mg g·(-1)和19.7mg g·(-1)。改性高岭石以吸热方式与Co(II)相互作用,但所有其他相互作用均为放热反应。在所有情况下,吉布斯能量的降低表明自发吸附。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号