首页> 外文期刊>Applied clay science >Competitive sorption/desorption of Zn, Cd, Pb, Ni, Cu, and Cr by clay-bearing mining wastes
【24h】

Competitive sorption/desorption of Zn, Cd, Pb, Ni, Cu, and Cr by clay-bearing mining wastes

机译:含粘土采矿废物对锌,镉,铅,镍,铜和铬的竞争性吸附/解吸

获取原文
获取原文并翻译 | 示例
           

摘要

The competitive sorption-desorption of trace metal ions by kaolinite-bearing coal mining wastes in Upper Silesia and by smectite-bearing waste from a basalt quarry in Lower Silesia, both in Poland, were studied. Generally, at higher clay contents, the sorption on both kaolinite wastes followed the same sequence of efficiency: Cr ~ Zn > Pb > Cu > Ni > Cd, while the sequence for the smectite waste was Zn > Pb > Cd > Cu > Ni > Cr. The retention of the metal ions followed the same sequence for all day-bearing wastes: Cr>Pb>Cu>Zn>Ni>Cd. The sorption of the day-bearing coal mining wastes was considerable, though the kaolinite and illite were the main components. There were no significant differences between both kaolinite-bearing wastes in the sorption/desorption capadty. In spite of this, the highest pH (approx. 8) of the KaW-1 kaolinite-bearing waste and the presence of iron (hydr)oxides may be crurial in explaining the observed differences. The day waste samples showed similar retention for all metal ions except Pb. The highest retention was observed for Cr. Lead showed a lower retention, and the difference among clay wastes was noticeable. The amounts of metal ions sorbed and desorbed by the day wastes depended on the type of clay waste, its composition and grain size, trace metal type and concentration, solid/solution (s/l) ratio, pH and the presence of other trace metal ions. It is concluded that in addition to adsorption, predpitation controlled the removal of trace metal ions from multimetal solutions.
机译:研究了波兰上西里西亚含高岭石的煤炭开采废物和下西里西亚含玄武岩采石场的蒙脱石废物对痕量金属离子的竞争性吸附-解吸。通常,在粘土含量较高时,两种高岭石废物的吸附效率顺序相同:Cr〜Zn> Pb> Cu> Ni> Cd,而蒙脱石废物的吸附顺序为Zn> Pb> Cd> Cu> Ni>铬对于所有含日废物,金属离子的保留遵循相同的顺序:Cr> Pb> Cu> Zn> Ni> Cd。尽管高岭石和伊利石是主要成分,但对日间采煤废物的吸附相当可观。两种含高岭石的废物在吸附/解吸能力上没有显着差异。尽管如此,在解释所观察到的差异时,可能最关键的是KaW-1高岭石废料的最高pH值(约8)和(铁)氧化物的存在。当日废物样品对除Pb以外的所有金属离子均显示相似的保留率。 Cr的保留率最高。铅的保留率较低,而粘土废物之间的差异也很明显。日间废物吸收和解吸的金属离子的量取决于粘土废物的类型,其组成和粒度,痕量金属的类型和浓度,固/溶液(s / l)比,pH值以及其他痕量金属的存在离子。结论是,除吸附外,沉淀还控制了多金属溶液中痕量金属离子的去除。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号