Durability performance of concrete containing Saudi natural pozzolans as supplementary cementitious material

机译:混凝土的耐久性含有沙特天然波佐醇的辅助胶凝材料

获取原文
获取原文并翻译 | 示例
           

摘要

This paper reports an experimental investigation conducted to evaluate the durability performance of concrete mixtures prepared utilizing blends of Type I Portland cement (OPC) and natural pozzolans (NPs) obtained from three different sources in Saudi Arabia. The control concrete mixture containing OPC alone as the binder and three concrete mixtures incorporating NPs were prepared keeping water/binder ratio of 0.4 (by weight), binder content of 370 kg/m(3), and fine/total aggregate ratio of 0.38 (by weight) invariant. The compressive strength and durability properties that included depth of water penetration, depth of carbonation, chloride diffusion coefficient, and resistance to reinforcement corrosion and sulfate attack were determined. Results of this study indicate that at all ages, the compressive strength of NP-admixed concrete mixtures was slightly less than that of the concrete containing OPC alone. However, the concrete mixtures containing NP exhibited lower depth of water penetration and chloride diffusion coefficient and more resistance to reinforcement corrosion and sulfate attack as compared to OPC. NP-admixed concrete showed relatively more depth of carbonation than OPC when subjected to accelerated carbonation. The results of this investigation indicates the viability of utilizing of Saudi natural pozzolans for improving the durability characteristics of concrete subjected to chloride and sulfate exposures.
机译:本文报道了一种实验研究,以评估利用来自沙特阿拉伯的三种不同来源的I型Portland水泥(OPC)和天然火山虫(NPS)的混合物制备的混凝土混合物的耐久性性能。将含有OPC的控制混凝土混合物作为粘合剂和包含NPS的三种混凝土混合物,保持水/粘合剂比0.4(重量),粘合剂含量为370kg / m(3),细/总骨料比为0.38(按重量)不变。确定了施加强度和耐久性,包括水渗透深度,碳化深度,氯化物扩散系数和对增强腐蚀和硫酸盐发作的抗性。该研究的结果表明,在所有年龄段,NP-混合混凝土混合物的抗压强度略小于含有OPC的混凝土的抗压强度。然而,与OPC相比,含有NP的混凝土混合物表现出较低的水渗透和氯化物扩散系数和更高的增强腐蚀和硫酸盐发作。当受到加速碳酸化时,NP-混合混凝土显示比OPC相对较长的碳酸化。该研究的结果表明,利用沙特天然火山唑来改善氯化物和硫酸盐曝光的混凝土耐久性特征的可行性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号