Honeycomb-Like Spherical Cathode Host Constructed from Hollow Metallic and Polar Co_9S_8 Tubules for Advanced Lithium-Sulfur Batteries

机译:由空心金属和极性Co_9S_8小管构造的蜂窝状球形阴极主体,用于高级锂硫电池

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The practical application of lithium-sulfur (Li-S) batteries remains remote because of rapid capacity fade caused by the low conductivity of sulfur, dissolution of intermediate lithium polysulfides, severe volumetric expansion, and slow redox kinetics of polysulfide intermediates. Here, to address these obstacles, a new sulfiphilic and highly conductive honeycomb-like spherical cathode host constructed from hollow metallic and polar Co9S8 tubes is designed. Co9S8 can effectively bind polar polysulfides for prolonged cycle life, due to the strong chemisorptive capability for immobilizing the polysulfide species. The hollow structure, as the sulfur host, can further prevent polysulfide dissolution and offer sufficient space to accommodate the necessary volume expansion. Well-aligned tubular arrays provide a conduit for rapid conduction of electrons and Li-ions. More importantly, the experimental results and theoretical calculations show that Co9S8 plays an important catalytic role in improving the electrochemical reaction kinetics. When used as cathode materials for Li-S batteries, the S@Co9S8 composite cathode exhibits high capacity and an exceptional stable cycling life demonstrated by tests of 600 cycles at 1 C with a very low capacity decay rate of only approximate to 0.026% per cycle.
机译:由于硫的低电导率,中间的多硫化锂中间物的溶解,严重的体积膨胀以及多硫化物中间体的氧化还原动力学缓慢,锂硫(Li-S)电池的实际应用仍然遥遥无期。在这里,为解决这些障碍,设计了一种由空心金属和极性Co9S8管构成的新的亚磺酸和高导电性蜂窝状球形阴极主体。由于具有强大的固定化多硫化物种类的化学吸附能力,Co9S8可以有效地结合极性多硫化物,从而延长循环寿命。中空结构作为硫主体,可以进一步防止多硫化物溶解,并提供足够的空间来容纳必要的体积膨胀。排列良好的管状阵列为快速传导电子和锂离子提供了导管。更重要的是,实验结果和理论计算表明,Co9S8在改善电化学反应动力学方面起着重要的催化作用。当用作Li-S电池的正极材料时,S @ Co9S8复合正极表现出高容量和出色的稳定循环寿命,通过在1 C下进行600次循环测试证明,极低的容量衰减率仅为每个循环约0.026% 。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号