Shear Bond Strength of Acidic Primer, Light-Cure Glass Ionomer, Light-Cure and Self Cure Composite Adhesive Systems - An In Vitro Study

机译:酸性底漆,光固化玻璃离聚物,光固化和自固化复合胶粘剂体系的剪切粘结强度-体外研究

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Background: The purpose of this study was to determine shear bond strength and the effect on the bracket/ adhesive failure mode when an acidic primer and other etchants were used to condition the enamel surface before bonding.Materials & Methods: Group I: Brackets bonded with Ultimate cure-on-light Light-cure composite adhesive system. Group II: Brackets bonded with Ortho-one no-mix. Self-cure composite adhesive system. Group III: Brackets bonded with Light-cure glass ionomer adhesive system. Group IV: Brackets bonded with Transbond plus self etching primer.Results: The results of this study indicated that the shear bond strength when using Transbond plus self etching primer showed the highest bond strength Group- IV(8.69 2.54 MPa) followed by Ultimate cure-on-light Group-I (8.62 1.84 MPa), Ortho-one no-mix (Bisco Inc. USA)Group-II (8.07 1.72 MPa), and least bond strength was seen in G.C. Fuji Ortho L.C. Group-III (6.01 1.6) MPaConclusion: Use of self etching primer saves chairside time and satisfactory high bond strength was obtained. Care should be taken during debonding of ceramic bracketsHow to cite this article: Reddy K D, Kishore M S V, Safeena S. Shear Bond Strength of Acidic Primer, Light-Cure Glass Ionomer, Light-Cure and Self Cure Composite Adhesive Systems - An In Vitro Study. J Int Oral Health 2013; 5(3):73-78.
机译:背景:本研究的目的是确定在粘结前使用酸性底漆和其他蚀刻剂调节釉质表面时的剪切粘结强度以及对托架/粘合剂破坏模式的影响。材料和方法:第一组:用Ultimate-light-光固化光固化复合胶粘剂系统粘结的支架。第II组:用Ortho-one no-mix粘合的支架。自固化复合胶系统。第三组:用光固化玻璃离聚物粘合剂体系粘合的支架。 IV组:用Transbond加自蚀底漆粘结的支架。结果:研究结果表明,使用Transbond加自蚀底漆的剪切粘结强度最高,IV-组(8.69 2.54) MPa),其次是Ultimate-I-O光固化(8.62 1.84 MPa),Ortho-one no-mix(美国Bisco Inc.)II组(8.07 1.72 MPa),在GC中观察到的粘结强度最低富士Ortho L.C. III组(6.01 1.6)MPa 结论:使用自蚀刻底漆可节省椅子旁的时间,并获得令人满意的高粘结强度。剥离陶瓷托槽时应注意如何引用本文:Reddy KD,Kishore MSV,SafeenaS。酸性底漆,光固化玻璃离聚物,光固化和自固化的剪切粘结强度复合胶粘剂系统-体外研究。 《国际口腔卫生杂志》 2013; 5(3):73-78。