Objective. This study was designed to evaluate the effect of nano-tricalcium phosphate (n-TCP) and nanohydroxyapatite (n-HAP) on prevention of restaining of enamel after dental bleaching. Methods. Forty bovine incisors were bleached with 20% carbamide peroxide for two weeks. Afterward, they were divided into five groups based on remineralization solution: no treatment (control), 10% n-TCP, 5% n-TCP, 10% n-HAP, and 5% n-HAP. Each group was daily immersed for 10 minutes in the restaining solution (tea) and for 3 minutes in the remineralization agent, respectively. This protocol was repeated for five days. Subsequently, three digital photographs (baseline, after bleaching, and after restaining) were analyzed by Adobe Photoshop software. The obtained L , a , b , and ΔE parameters were compared using ANOVA and Wilcoxon and Bonferroni tests. Results. After bleaching, there were significant changes in tooth colors (P < 0.001) while, after restaining and immersion in remineralization solutions, there were no significant differences in L , a , and b values of different groups (P > 0.05). However, ΔE of 10% TCP was significantly lower than the control (P = 0.02) while there were no significant differences between the other groups (P > 0.05). Conclusion. 10% n-TCP could significantly maintain the resultant color and reconstruct the enamel structure after bleaching.
机译:目的。本研究旨在评估纳米磷酸三钙(n-TCP)和纳米羟基磷灰石(n-HAP)对预防牙齿漂白后牙釉质残留的作用。方法。用20%的过氧化脲将40个牛切牙漂白两周。然后,根据矿化溶液将其分为五组:无处理(对照),10%n-TCP,5%n-TCP,10%n-HAP和5%n-HAP。每组每天分别在保持液(茶)中浸泡10分钟,在再矿化剂中浸泡3分钟。重复该方案五天。随后,通过Adobe Photoshop软件分析了三张数码照片(基线,漂白后和保留后)。使用方差分析,Wilcoxon和Bonferroni测试比较获得的L ,a ,b 和ΔE参数。结果。漂白后,牙齿的颜色发生了显着变化(P <0.001),而在保留和浸入矿化溶液后,L * ,a 没有显着差异。 ,以及不同组的b 值( P E 显着低于对照组( P = 0.02),而其他两组之间( P 结论。 10%的n-TCP可以显着保持所得颜色并在漂白后重建瓷釉结构。