Effects of Preparation Methods on the Thermoelectric Performance of SWCNT/Bi2Te3 Bulk Composites

机译:制备方法对SWCNT / Bi2Te3本体复合材料热电性能的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Single-walled carbon nanotube (SWCNT)/Bi Te composite powders were fabricated via a one-step in situ reductive method, and their corresponding bulk composites were prepared by a cold-pressing combing pressureless sintering process or a hot-pressing process. The influences of the preparation methods on the thermoelectric properties of the SWCNT/Bi Te bulk composites were investigated. All the bulk composites showed negative Seebeck coefficients, indicating n-type conduction. A maximum power factor of 891.6 μWm K at 340 K was achieved for the SWCNT/Bi Te bulk composites with 0.5 wt % SWCNTs prepared by a hot-pressing process, which was ~5 times higher than that of the bulk composites (167.7 μWm K at 300 K) prepared by a cold-pressing combing pressureless sintering process, and ~23 times higher than that of the bulk composites (38.6 μWm K at 300 K) prepared by a cold-pressing process, mainly due to the enhanced density of the hot-pressed bulk composites.
机译:采用单步原位还原法制备了单壁碳纳米管(SWCNT)/ Bi Te复合粉末,并通过冷压梳理无压烧结或热压工艺制备了相应的块状复合材料。研究了制备方法对SWCNT / Bi Te本体复合材料热电性能的影响。所有块状复合材料均显示负塞贝克系数,表明其为n型导电。通过热压工艺制备的具有0.5 wt%SWCNT的SWCNT / Bi Te块状复合材料在340 K时达到891.6μWmK的最大功率因数,比块状复合材料(167.7μWmK)高约5倍300 K)是通过冷压精梳无压烧结工艺制备的,比通过冷压方法制备的本体复合材料(300 K时为38.6μWmK)高约23倍。热压块状复合材料。