首页> 美国卫生研究院文献>Materials >Preparation of Black Ceramic Tiles Using Waste Copper Slag and Stainless Steel Slag of Electric Arc Furnace
【2h】

Preparation of Black Ceramic Tiles Using Waste Copper Slag and Stainless Steel Slag of Electric Arc Furnace

机译:用废铜渣和电弧炉不锈钢渣制备黑色瓷砖

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Copper slag and stainless steel slag of Electric Arc Furnace (EAF) are two typical metallurgical solid wastes, which contain a large number of valuables, such as Fe, Cr, and Cu. The transition metal elements in the waste slags, such as Cr and Fe, can be recycled as the coloring ions in the black ceramic tile. In this study, the Fe/Cr molar ratio in the raw materials of copper slag and stainless steel slag was adjusted, and the black ceramic tile was subsequently prepared by sintering. The results show that the optimum process parameters for the preparation of black ceramic tiles are the Fe/Cr molar ratio of 2.0, the sintering temperature of 1150 °C, and the sintering time of 30 min. The compressive strength of the black ceramic tile at optimum sintering conditions exceeds the minimum compressive strength of the Chinese national standard for standard polished tiles, and the concentrations of harmful elements, for example, Cr, Cu, Ni, As, Zn, Pb, and Cr(VI) are within the regulation thresholds specified by the Chinese national standard.
机译:电弧炉(EAF)的铜渣和不锈钢渣是两种典型的冶金固体废物,其中含有大量的贵重金属,例如铁,铬和铜。废渣中的过渡金属元素(例如Cr和Fe)可以作为黑色瓷砖中的着色离子进行回收利用。在这项研究中,调整了铜渣和不锈钢渣原料中的Fe / Cr摩尔比,然后通过烧结制备了黑色瓷砖。结果表明,制备黑色瓷砖的最佳工艺参数为Fe / Cr摩尔比为2.0,烧结温度为1150°C,烧结时间为30 min。在最佳烧结条件下,黑色瓷砖的抗压强度超过了中国国家标准抛光砖的最低抗压强度,以及有害元素的浓度,例如Cr,Cu,Ni,As,Zn,Pb和六价铬在中国国家标准规定的规定阈值内。