A field study was conducted to estimate the amount of Cr, Mn, and Ni deposited in the respiratory system of 44 welders in two facilities. Each worker wore a nanoparticle respiratory deposition (NRD) sampler during gas metal arc welding (GMAW) of mild and stainless steel and flux-cored arc welding (FCAW) of mild steel. Several welders also wore side-by-side NRD samplers and closed-face filter cassettes for total particulate samples. The NRD sampler estimates the aerosol's nano-fraction deposited in the respiratory system. Mn concentrations for both welding processes ranged 2.8–199 μg/m3; Ni concentrations ranged 10–51 μg/m3; and Cr concentrations ranged 40–105 μg/m3. Cr(VI) concentrations ranged between 0.5–1.3 μg/m3. For the FCAW process the largest concentrations were reported for welders working in pairs. As a consequence this often resulted in workers being exposed to their own welding fumes and to those generated from the welding partner. Overall no correlation was found between air velocity and exposure (R2 = 0.002). The estimated percentage of the nano-fraction of Mn deposited in a mild-steel-welder's respiratory system ranged between 10 and 56%. For stainless steel welding, the NRD samplers collected 59% of the total Mn, 90% of the total Cr, and 64% of the total Ni. These results indicate that most of the Cr and more than half of the Ni and Mn in the fumes were in the fraction smaller than 300 nm.
机译:进行了一项现场研究,以估算沉积在两个工厂的44名焊工的呼吸系统中的Cr,Mn和Ni的含量。在低碳钢和不锈钢的气体保护金属电弧焊(GMAW)和低碳钢的药芯焊丝(FCAW)焊接过程中,每个工人都佩戴了纳米颗粒呼吸沉积(NRD)采样器。几名焊工还佩戴了并排的NRD采样器和封闭式过滤器盒,以收集全部颗粒样品。 NRD采样器估计沉积在呼吸系统中的气溶胶的纳米级分。两种焊接工艺中的锰浓度范围为2.8-199μg/ m 3 ;镍的浓度范围为10-51μg/ m 3 ; Cr的浓度范围为40-105μg/ m 3 。 Cr(VI)的浓度范围为0.5–1.3μg/ m 3 。对于FCAW工艺,成对工作的焊工报告的最大浓度。结果,这常常导致工人暴露于他们自己的焊接烟雾和由焊接伙伴产生的烟雾中。总体上没有发现风速与暴露之间的相关性(R 2 = 0.002)。在低碳钢焊工的呼吸系统中沉积的锰纳米级分的估计百分比在10%到56%之间。对于不锈钢焊接,NRD采样器收集了59%的Mn,90%的Cr和64%的Ni。这些结果表明,烟气中的大部分Cr和一半以上的Ni和Mn含量均小于300 nm。