A simple microplasma method was used to synthesize cuprous oxide (Cu2O) nanoparticles in NaCl–NaOH–NaNO3 electrolytic system. Microplasma was successfully used as the cathode and copper plate was used as the anode. The Cu2O products are characterized by X–ray powder diffraction (XRD), field emission scanning electron microscope (FESEM) and transmission electron microscope (TEM). The results show that the morphology of Cu2O nanocrystals obtained by this technology is mainly dependent on the electrolytic media, stirring, current density and reaction temperature. The uniform and monodisperse sphere Cu2O nanoparticles with the size about 400 ~ 600 nm can be easily obtained in H2O–ethylene glycol mix–solvent (volume ratio 1:1) and appropriate current density with stirring at room temperature. In addition, the possible mechanism has been reported in the article. And the average energy consumed in producing 1 g Cu2O nanoparticles is 180 kJ. For the flexibility and effectiveness of this microplasma technology, it will have broad application prospects in the realm of nanoscience, energy and environment.
机译:一种简单的微等离子体方法被用于在NaCl–NaOH–NaNO3电解系统中合成氧化亚铜(Cu2O)纳米颗粒。微等离子体成功用作阴极,铜板用作阳极。 Cu2O产品通过X射线粉末衍射(XRD),场发射扫描电子显微镜(FESEM)和透射电子显微镜(TEM)进行表征。结果表明,该技术制得的Cu2O纳米晶的形貌主要取决于电解液,搅拌,电流密度和反应温度。在H2O-乙二醇混合溶剂(体积比为1:1)和室温下适当的电流密度下,可以轻松获得大小约为400〜600 nm的均匀且分散的球形Cu2O纳米颗粒。此外,文章中还报告了可能的机制。生产1 g Cu2O纳米颗粒所消耗的平均能量为180 kJ。由于这种微等离子体技术的灵活性和有效性,它将在纳米科学,能源和环境领域具有广阔的应用前景。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号