The impact of AEO7 surfactant on the corrosion inhibition of carbon steel (C-steel) in 0.5 M HCl solution at temperatures between 20 °C and 50 °C was elucidated using weight loss and different electrochemical techniques. The kinetics and thermodynamic parameters of the corrosion and inhibition processes were reported. The corrosion inhibition efficiency (IE%) improved as the concentration of AEO7 increased. In addition, a synergistic effect was observed when a concentration of 1 × 10−3 mol L−1 or higher of potassium iodide (KI) was added to 40 µmol L−1 of the AEO7 inhibitor where the corrosion IE% increased from 87.4% to 99.2%. Also, it was found that the adsorption of AEO7 surfactant on C-steel surface followed the Freundlich isotherm. Furthermore, electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization measurements indicated that AEO7 was physically adsorbed on the steel surface. The surface topography was examined using an optical profilometer, an atomic force microscope (AFM), and a scanning electron-microscope (SEM) coupled with an energy dispersion X-ray (EDX) unit. Quantum chemical calculations based on the density functional theory were performed to understand the relationship between the corrosion IE% and the molecular structure of the AEO7 molecule.
机译:使用重量损失和不同的电化学技术,阐明了AEO7表面活性剂对0.5 M HCl溶液中碳钢(C-钢)在20 C和50 C之间的温度下的腐蚀抑制的影响。报道了腐蚀和抑制过程的动力学和热力学参数。随着AEO7浓度的增加,缓蚀效率(IE%)提高。另外,当在40 µmol L <10中添加1×10 -3 mol L -1 或更高浓度的碘化钾(KI)时,可观察到协同作用。 AEO7抑制剂的sup> -1 ,腐蚀IE%从87.4%增加到99.2%。另外,发现AEO7表面活性剂在碳钢表面上的吸附遵循弗氏等温线。此外,电化学阻抗谱(EIS)和电位动力学极化测量表明,AEO7物理吸附在钢表面上。使用光学轮廓仪,原子力显微镜(AFM)和带有能量色散X射线(EDX)单元的扫描电子显微镜(SEM)检查表面形貌。进行了基于密度泛函理论的量子化学计算,以了解腐蚀IE%与AEO7分子的分子结构之间的关系。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号