摘要

The main objective of this work was to study the structural viability of using small-diameter logs of Uruguayan Loblolly/Slash pine, mainly from thinning operations, to design cross-laminated timber (CLT) panels. A visual grade named “CTH” (coniferous thinning) was proposed, and 45 specimens of sawn timber boards were tested, resulting in 51% lower bending strength than that of the minimum strength class C14. Subsequently, 20 CLT panels were manufactured and experimentally tested, the results showed that the bending strength of the CLT panels was 43% above that of the individual layers. Additionally, the structural performance of the CLT panels for use in floors was calculated, and the thickness-span relationship depending on strength class and imposed load are presented. Results showed than the use of CTH timber to design CLT floors implies a volume (m3/m2) 17% higher than that using C24 timber.
机译:这项工作的主要目的是研究使用小直径原木(主要是来自减薄作业)的乌拉圭火炬松/深松的原木来设计交叉层压木板(CLT)的结构可行性。提出了一个视觉等级“ CTH”(针叶薄化),并测试了45个锯材木板样品,其弯曲强度比最低强度等级C14低51%。随后,制造了20个CLT面板并进行了实验测试,结果表明CLT面板的弯曲强度比各个层的弯曲强度高43%。另外,计算了用于地板的CLT面板的结构性能,并给出了取决于强度等级和施加载荷的厚度与跨度的关系。结果表明,与使用CTH木材设计CLT地板相比,其体积(m 3 / m 2 )比使用C24木材高17%。