摘要

The deformation and failure kinetics of polyamide 6 samples prepared by several thermal histories were investigated by tests at different temperatures and relative humidities. PA6 samples were produced in quiescent condition and multiple cooling procedure. A characterization was performed to investigate the effect of the different thermal histories and the effect of hydration on both structures and glass transition temperature. The mechanical properties were investigated by tensile and creep tests at different temperatures and relative humidity. In order to describe the experimental results, the Ree–Eyring equation, modified with the “apparent temperature”, was employed. In addition, the results of time-to-failure (creep tests) were described by the use of the “critical strain” concept. Eventually, a link between the Eyring theory and the structure evolution was made, i.e., a relation between the rate factors and the average lamellar thickness.
机译:通过在不同温度和相对湿度下的测试,研究了由多种热史制备的聚酰胺6样品的变形和破坏动力学。 PA6样品在静态条件下和多次冷却过程中生产。进行表征以研究不同热历史的影响以及水合对结构和玻璃化转变温度的影响。通过在不同温度和相对湿度下的拉伸和蠕变试验研究了机械性能。为了描述实验结果,使用了用“表观温度”修改的Ree-Eyring方程。此外,使用“临界应变”概念描述了失效时间(蠕变测试)的结果。最终,在Eyring理论与结构演变之间建立了联系,即速率因子与平均层状厚度之间的关系。