Eco-Friendly and Highly Efficient Enzyme-Based Wool Shrinkproofing Finishing by Multiple Padding Techniques

机译:采用多种填充技术的环保型高效酶基羊毛防缩整理剂

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Wool fibers usually need shrinkproofing finishing. The enzyme process is an eco-friendly technology but the traditional exhaustion treatment usually takes excessive time. This study developed a novel multiple padding shrinkproofing process of wool with Savinase 16L and an organic phosphine compound {[HO(CH2)n]3P, n ∈ (1, 10)}. SEM and XPS analyses were employed to compare the wool treated respectively by exhaustion and by padding to reveal the effect of multiple padding. The results showed that treated wool fiber achieved the requirement of machine-washable (area shrinkage less than 8% according to standard TM 31 5 × 5A) in 2.5 min by the padding process. The padding process can control the adsorbance of enzyme on wool, which makes treatment more uniform and avoids strong damage of the wool. Also, the removal efficiency of the disulfide bond was about 15 times as much as in the exhaustion treatment in 2.5 min. The average catalytic rate of the padding process was 14 times faster than the exhaustion process, and the process time (2.5 min) decreased by 32.5 min compared with the exhaustion process (35 min). Multiple padding techniques can achieve continuous production and replace the environmentally harmful chlorination process. Our results provide the underlying insights needed to guide the research of the enzyme process application.
机译:羊毛纤维通常需要防缩整理。酶法是一种环保技术,但是传统的精疲力尽处理通常会花费大量时间。这项研究开发了一种新型的用Savinase 16L和有机膦化合物{[HO(CH2)n] 3P,n∈(1,10)}的羊毛多重填充防缩工艺。使用SEM和XPS分析来比较分别用精疲力尽和填充处理的羊毛,以揭示多重填充的效果。结果表明,经过处理的羊毛纤维在填充过程中在2.5分钟内达到了可机洗的要求(根据标准TM 31 5×5A,面积收缩率小于8%)。填充过程可以控制酶在羊毛上的吸附,从而使处理更均匀并避免对羊毛造成强烈损害。另外,二硫键的去除效率是2.5分钟内的疲劳处理的约15倍。填充过程的平均催化速率比排气过程快14倍,与排气过程(35分钟)相比,处理时间(2.5分钟)减少了32.5分钟。多种填充技术可实现连续生产,并取代对环境有害的氯化工艺。我们的结果提供了指导酶法应用研究的基础见识。