Hydrophobic Y-zeolite (SiO2/Al2O3 = 810) and TiO2 composite photocatalysts were designed by using two different types of TiO2 precursors, i.e., titanium ammonium oxalate and ammonium hexafluorotitanate. The porous structure, surface property and state of TiO2 were investigated by various characterization techniques. By using an ammonium hexafluorotitanate as a precursor, hydrophobic modification of the Y-zeolite surface and realizing visible light sensitivity was successfully achieved at the same time after calcination at 773 K in the air. The prepared sample still maintained the porous structure of Y-zeolite and a large surface area. Highly crystalline anatase TiO2 was also formed on the Y-zeolite surface by the role of fluorine in the precursor. The usages of ammonium hexafluorotitanate were effective for the improvement of the photocatalytic performance of the composite in the degradation of 2-propanol in the gas phase under UV and visible light (λ > 420 nm) irradiation.
机译:通过使用两种不同类型的TiO2前驱体,即草酸钛铵和六氟钛酸铵,设计了疏水性Y沸石(SiO2 / Al2O3 = 810)和TiO2复合光催化剂。通过各种表征技术研究了TiO2的多孔结构,表面性质和状态。通过使用六氟钛酸铵作为前体,在空气中于773 K煅烧后,成功地实现了Y沸石表面的疏水改性并实现了可见光灵敏度。所制备的样品仍保持Y型沸石的多孔结构和较大的表面积。由于氟在前体中的作用,Y沸石表面还形成了高度结晶的锐钛矿型TiO2。六氟钛酸铵的使用有效地改善了复合物在紫外和可见光(λ> 420 nm)照射下气相中2-丙醇降解中的光催化性能。