The investigation presented here features the design of a cleaner and greener chemical process for the conversion of industrial wastes into super-oxidizing materials. The waste of interest is the iron sulfate heptahydrate (FeSO4·7H2O) mainly generated through the sulfate route used for titanium dioxide industrial production. The products of this transformation process are alkali ferrates (A2FeO4, A = Na, K) containing iron in its hexavalent state and considered as powerful oxidants characterized by properties useful for cleaning waters, wastewaters, and industrial effluents. The proposed process includes two steps: (i) The first step consisting of the pre-mixing of two solids (AOH with FeSO4·xH2O) in a rotary reactor allowing the coating of iron sulfate in the alkali hydroxides through solid–solid reactions; and (ii) the second step involves the synthesis of alkali ferrates in a fluidized bed by oxidation of the single solid obtained in the first step in diluted chlorine. The chemical synthesis of alkali ferrates can be carried out within a timeframe of a few minutes. The usage of a fluidized bed enhanced the energy and mass transfer allowing a quasi-complete control of the ferrate synthesis process. The alkali ferrate synthesis process described here possesses many characteristics aligned with the principles of the “green chemistry”.
机译:本文介绍的研究的特点是设计一种更清洁,更环保的化学工艺,以将工业废料转化为超氧化性材料。感兴趣的废物是主要通过用于二氧化钛工业生产的硫酸盐途径产生的七水合硫酸铁(FeSO4·7H2O)。此转化过程的产物是六价态含铁的碱金属高铁酸盐(A2FeO4,A = Na,K),被认为是强氧化剂,其特征在于可用于清洁水,废水和工业废水。拟议的过程包括两个步骤:(i)第一步是在旋转反应器中将两种固体(AOH与FeSO4·xH2O)进行预混合,使硫酸铁通过固-固反应涂覆在碱金属氢氧化物中; (ii)第二步涉及在流化床中通过在稀释的氯气中氧化第一步中获得的单一固体来合成碱金属高铁酸盐。高铁酸碱金属盐的化学合成可以在几分钟内完成。流化床的使用增强了能量和质量传递,从而允许对高铁酸盐合成过程进行准完全控制。本文所述的碱金属高铁酸盐合成方法具有许多符合“绿色化学”原理的特征。