Objectives. To evaluate the surface hardness of two light-cured resin cements polymerized under different ceramic discs. Methods. 40 experimental groups of 2 light-cured resin cement specimens (Variolink Veneer and NX3) were prepared and polymerized under 5 different ceramic discs (IPS e.max Press HT, LT, MO, HO, and Cercon) of 4 thicknesses (0.5, 1.0, 1.5, and 2.0 mm), Those directly activated of both resin cements were used as control. After light activation and 37°C storage in an incubator, Knoop hardness measurements were obtained at the bottom. The data were analyzed with three-way ANOVA, t-test, and one-way ANOVA. Results. The KHN of NX3 was of significantly higher than that of Variolink Veneer (P < 0.05). The KHN of resin cement polymerized under different ceramic types and thicknesses was significant difference (P < 0.05). Conclusion. Resin cements polymerized under different ceramic materials and thicknesses showed statistically significant differences in KHN.
机译:目标。为了评估在不同陶瓷盘下聚合的两种光固化树脂胶粘剂的表面硬度。方法。制备了40个实验组的2个光固化树脂水泥样品(Variolink Veneer和NX3),并在5种不同厚度为0.5、1.0、1.0的陶瓷盘(IPS e.max Press HT,LT,MO,HO和Cercon)下聚合(分别为1.5和2.0?mm),两种树脂水泥直接活化的树脂均用作对照。在激活光并在培养箱中37°C保存后,在底部获得努氏硬度测量值。使用三向ANOVA,t检验和单向ANOVA分析数据。结果。 NX3的KHN明显高于Variolink单板的KHN(P <0.05)。在不同陶瓷类型和厚度下聚合的树脂水泥的KHN有显着差异(P <0.05)。结论。在不同陶瓷材料和厚度下聚合的树脂水泥在KHN中显示出统计学上的显着差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号