Cytotoxicity and Initial Biocompatibility of Endodontic Biomaterials (MTA and Biodentine™) Used as Root-End Filling Materials

机译:牙根生物材料(MTA和Biodentine™)用作根端填充材料的细胞毒性和初始生物相容性

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Objective. The aim of this study was to evaluate the cytotoxicity and cellular adhesion of Mineral Trioxide Aggregate (MTA) and Biodentine (BD) on periodontal ligament fibroblasts (PDL). Methods. PDL cells were obtained from nonerupted third molars and cultured; MTS cellular profusion test was carried out in two groups: MTA and BD, with respective controls at different time periods. Also, the LIVE/DEAD assay was performed at 24 h. For evaluation of cellular adhesion, immunocytochemistry was conducted to discern the expression of Integrin β1 and Vinculin at 12 h and 24 h. Statistical analysis was performed by the Kruskal-Wallis and Mann-Whitney U tests. Results. MTA and BD exhibited living cells up to 7 days. More expressions of Integrin β1 and Vinculin were demonstrated in the control group, followed by BD and MTA, which also showed cellular loss and morphological changes. There was a significant difference in the experimental groups cultured for 5 and 7 days compared with the control, but there was no significant statistical difference between both cements. Conclusions. Neither material was cytotoxic during the time evaluated. There was an increase of cell adhesion through the expression of focal contacts observed in the case of BD, followed by MTA, but not significantly.
机译:目的。这项研究的目的是评估对牙周膜成纤维细胞(PDL)的三氧化二矿骨料(MTA)和Biodentine(BD)的细胞毒性和细胞粘附性。方法。从未磨牙的第三磨牙获得PDL细胞并进行培养; MTS细胞灌注测试分为两组:MTA和BD,分别在不同的时间段进行对照。此外,LIVE / DEAD分析在24小时进行。为了评估细胞粘附性,进行了免疫细胞化学分析,以在12 h和24 Vinh区分整合素β1和Vinculin的表达。统计分析通过Kruskal-Wallis和Mann-Whitney U检验进行。结果。 MTA和BD可以显示长达7天的活细胞。在对照组中,整合素β1和Vinculin的表达更多,其次是BD和MTA,它们也显示细胞丢失和形态变化。与对照组相比,培养5天和7天的实验组有显着差异,但两种胶结剂之间无统计学差异。结论。在评估期间,两种材料均无细胞毒性。通过在BD的情况下观察到的焦点接触的表达,细胞粘附增加,随后是MTA,但没有显着增加。