High-temperature oxidation behavior of CeO_2-SiO_2/Ni-W-P composites

         

摘要

Ni-W-P matrix composites containing CeO2 and SiO2 nano-particles were prepared on common carbon steel surface by means of pulse electrodeposition,and the high-temperature oxidation behavior was investigated.The results show that when the oxidation time is controlled in 1 h,oxidation kinetics curve between oxidation mass gain rate and oxidation temperature of CeO2-SiO2/Ni-W-P composites accords with the index increasing law.When the oxidation temperature is controlled at 300℃,the kinetics curve between oxidation mass gain rate and oxidation time accords with the linear increasing law.The composites as-deposited are in the amorphous state and turn into the crystal state at 400℃.The microstructures of oxidation film on the composites will change from the compact state to the loose state with increasing oxidation temperature to 800℃.They are still continuous and compact,and there are no crackle,strip and falling-out.CeO2 and SiO2 nano-particles co-deposited into Ni-W-P alloy can improve the high-temperature oxidation resistance.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号