Environmentally friendly hybrid coating prepared by electro-deposition method at various seawater conditions

机译:

获取原文
获取原文并翻译 | 示例
       

摘要

The formation mechanism of calcareous deposit films in seawater involves an increase in pH at the metal/solution interface due to cathodic reactions, a raised carbonate ion concentration at the interface and precipitation of inorganic deposits such as CaCO3, Mg(OH)2. Environmentally friendly hybrid calcareous deposit films were formed by an electrochemical technique on steel substrates in various solution environments. And the influence of dissolved gas on formation of calcareous deposit films was investigated by scanning electron microscopy(SEM), energy dispersive spectroscopy(EDS) and X-ray diffractometry(XRD). Consequently, these results showed that formation of good overall calcareous deposited films by dissolved gas in seawater environments can be achieved by controlling the material composition and structure through effective use of electrochemical method.
机译:钙质沉积膜在海水中的形成机制涉及由于阴极反应而在金属/溶液界面上的pH增加,在界面处的升高的碳酸盐离子浓度和无机沉积物,例如CaCO 3,Mg(OH)2。环保型混合钙质钙质矿床通过各种溶液环境中的钢基材上的电化学技术形成。通过扫描电子显微镜(SEM),能量分散光谱(EDS)和X射线衍射法(XRD)研究了溶解气体对钙质沉积膜形成的影响。因此,这些结果表明,通过有效地使用电化学方法,可以通过控制材料组合物和结构来实现通过溶解气体形成良好的整体钙质沉积膜。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号