本文介绍了最新开发的超音速大气等离子喷涂(SAPS)技术制备细密柱晶结构热障涂层系统(SAPS-TBCs)的一些研究进展。由于SAPS喷涂15~45μm粒径的8YSZ氧化锆球形粉末在等离子射流中飞行速度约为400-450m/s,是普通大气等离子(APS:130~220m/s)2~3倍,可方便制备出体积分数达80%以上的薄片状细密柱晶结构TBC涂层,柱晶轴向长度可方便地控制在2~5μm,孔隙率可根据需要在1%~12%范围内调变。研究表明,这种结构的8YSZ-TBC涂层试样1100℃淬水热震循环可达400周次%The recently investigation progress of the thermal barrier coating(TBC) with fine columnar grains was fabricated by a newly developed technology which was called supersonic atmospheric plasma spraying(SAPS).The in-flight rate of molten particles of 8% Y2O